jubingxikangliefangshenduanxianweishicaiyongxianweijijubingxiweiyuanliao,jingteshugongyijiagongchulierxingchengdegaoqiangdushuzhuangdansiyoujixianwei,qiguyoudenaiqiangsuan,naiqiangjian,ruodaorexing,juyoujiqiwendingdehuaxuexingneng。jiarushajianghuohunningtuzhongkeyouxiaodekongzhishajiang、hunningtuzaichuqisuxingshousuojieduanzhongyouwendubianhuadengyinsuyinqideweiliefeng,fangzhijiyizhiliefengdexingchengjifazhan,dadagaishanhunningtudezuliekangshenxingneng,kangchongjijikangzhennengli,keyiguangfandeshiyongyudixiagongchengfangshui,gongyeminyongjianzhugongchengdewumian、牆體、地坪、水池、地下室,以及道路和橋梁等工程中。是砂漿、混凝土工程抗裂,防滲,耐磨的新型理想材料。
針(zhen)對(dui)國(guo)內(nei)幹(gan)粉(fen)建(jian)材(cai)行(xing)業(ye)的(de)實(shi)際(ji)需(xu)求(qiu),公(gong)司(si)專(zhuan)門(men)組(zu)織(zhi)技(ji)術(shu)力(li)量(liang)攻(gong)關(guan)了(le)纖(xian)維(wei)表(biao)麵(mian)改(gai)性(xing)技(ji)術(shu),推(tui)出(chu)保(bao)溫(wen)砂(sha)漿(jiang)專(zhuan)用(yong)的(de)聚(ju)丙(bing)烯(xi)短(duan)纖(xian)維(wei),深(shen)受(shou)廣(guang)大(da)客(ke)戶(hu)好(hao)評(ping)!
■物理參數
|
纖維類型 |
束狀單絲 |
密度 |
0.91g/cm3 |
|
當量直徑 |
18~48 μm |
長度 |
3、6、9、12、15、54mm 可根據用戶要求任意切割 |
|
抗拉強度 |
≥500MPa |
彈性模量 |
≥3850MPa |
|
斷裂伸長率 |
10~28% |
抗酸堿性 |
極高 |
|
熔點 |
160~180℃ |
燃點 |
580℃ |
■主要功能:
作為混凝土的次要加強筋材料,海能高聚丙烯纖維可大大提高其抗裂、抗滲、抗衝擊、抗震、抗凍、抗衝磨、抗爆裂、抗老化性能及和易性、泵送性、保水性。
●阻止混凝土裂縫的產生
●提高混凝土的抗滲透性能
●提高混凝土的抗凍融性能
●提高混凝土的抗衝擊、抗折、抗疲勞、抗震性能
●改善混凝土的耐久性,抗老化性
●提高混凝土的耐火性能
■應用領域:
●混凝土剛性自防水結構:
地下室底板、側牆、頂板、屋麵現澆樓板、蓄水池等。抗裂、抗衝擊、抗磨損要求高的工程、水利工程、地鐵、機場跑道、港口碼頭、立交高架橋橋麵、橋墩、超長結構等。
●水泥砂漿:
內(外)牆粉刷、加氣混凝土抹灰、室內裝飾膩子及保溫砂漿。
●抗爆、耐火工程:
人防軍事工程、石油平台、煙囪、耐火材料等。
●噴射混凝土:
隧道、涵洞襯砌、薄壁結構、斜坡加固等。
■使用說明
●建議摻量:
普通抹麵砂漿建議每方砂漿摻量為:0.9~1.2kg
保溫砂漿建議每噸添加量為:1~3kg
混凝土建議每方混凝土摻量為:0.6~1.8kg(供參考)
●施工工藝及步驟
①根據每次攪拌混凝土的方量,按照配合比要求(或建議摻量)準確計量每次加入纖維的重量。
②砂石料備好後,將纖維加入。建議使用強製式攪拌機。將集料連同纖維一起加入攪拌機,但須注意應保證纖維加在集料之間,幹拌30秒左右,加入水後,濕拌30秒左右,使纖維充分分散。
③攪拌完成後隨即取樣,如纖維已均勻分散成單絲,則混凝土可投入使用,如果仍有成束纖維則延長攪拌時間20~30秒,即可使用。
④加入纖維的混凝土同普通混凝土施工及養護工藝完全相同。
|